The Forestry Forum
General Forestry => Drying and Processing => Topic started by: Brad_S. on September 10, 2007, 09:54:26 PM
I was going to call Nyle about this but since Don reads this forum and others may have had a similar problem, I thought I try here instead.
Ran 3 loads of cypress through a Nyle 200 and now the condensation fins are coated with an orange/rust colored gunk. My guess is it needs to be sprayed with a pitch remover and then pressure rinsed? Is there a better, less messy answer?